JM insulation Refractory Bricks

JM insulation refractory bricks ,it is combined with mullite as the main crystal phase and phase of the refractory material, with high bauxite clinker as the main raw material, adding high purity refractory powder, according to the requirements of products, to join the organic composite fillers, after pouring forming, high temperature firing of lightweight mullite stonework.

Share With:
JM insulation Refractory Bricks

JM insulation refractory bricks ,it is combined with mullite as the main crystal phase and phase of the refractory material, with high bauxite clinker as the main raw material, adding high purity refractory powder, according to the requirements of products, to join the organic composite fillers, after pouring forming, high temperature firing of lightweight mullite stonework.

JM insulation bricks has JM23 insulation bricks, JM26insulation bricks, JM28insulation bricks.

JM insulation bricks FEATURES:

1.Low thermal conductivity:Gives good thermal insulation, enabling the use of thinwalled constructions.

2.Low heat storage:Due to their light weight and low thermal conductivity, JM bricks absorb minimal heat, giving significant energy savings in cyclically-operated kilns.

3.High hot compressive strength

JM insulation bricks Application

JM insulation refractory bricks are widely used for heat-insulating purpose in many kinds of industrial furnace, electric furnace and metallurgical stove, Cracking furnace in petroleum, Hot blast furnace in metallurgy,Ceramic roller kiln, tunnel kiln, shuttle kiln for electrical porcelain, Pot furnace for glass industry, Inner lining of kinds of electrial furnaces and high temperature equipment.

JM insulation refractory bricks Specifications

ltem JM23 JM26 JM28 JM30 JM32
Temperature classification ,℃ 1260 1430 1540 1650 1760
Al2O3,% ≥ 37 58 67 74 77
Fe2O3,% ≤ 0.7 0.7 0.6 0.5 0.3
Bulk Density,g/cm 0.5 0.8 1.0 1.0 1.3
Cold crushing strength,Mpa ≥ 1 2 2 2 2
Bending strength,Mpa 2 2 2 2 4
Thermal Conductivity w/(m·k)average temperature 400,℃  ≤ 0.2 0.3 0.35 0.38 0.5
350℃ 0.18 0.27 0.32 0.38 0.49
600℃ 0.24 0.32 0.36 0.42 0.51

 

 

 